Jams,

When fabricating non-magnetic materials, I make cardboard or Masonite gussets and/or end plates and hot glue them to the detail parts to hold their position while I make my first tack welds. Then after the assembly is tacked and test fit, I use a heat gun to remove the hot glued pieces.


D-cel