Wow, first I've heard of a SPF with a glass/paint problem. I know on some boats it happens--called "blisters", pinholes to dinner plate size, caused by moisture intrusion(#1 cause), or improperly cleaning of mold release waxes, cure is usually stripping the glass, then reglassing, after a "drying" period if moisture is present in the glas. Usually fibreglas cars don't suffer the problems of boats. Could be that your car didn't get a through enough cleaning and sanding before being sent to the paint shop--rare but it could happen in a SPF.

Talk to a dealer and have them inspect the car.